@article { author = {shirzadi javid, ali akbar and ghoddousi, parviz and Zal Nezhad, ali and mirvalad, sajjad}, title = {Examining the effect of super-plasticizers on the rheology of self-consolidating concrete at various times and temperatures}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {1-12}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.12916.1355}, abstract = {Designing and developing rheological properties of self-compacting concrete is an important issue in concrete technology. This matter is because of the combination of varied needs in the fresh mode, extremely complexed mixture proportions, and its naturally low yield stress. Selection of chemical admixtures, especially super-plasticizers plays an important role in Designing of self-consolidating concrete (SCC). In this paper, the rheological properties of SCC samples made with various chemical admixtures in various mixing time and temperatures were examined. Super-plasticizers are strongly influenced by the ambient temperature, due to the fact that the temperature dependent on the hydration rate affects the absorbance rate of the super-plasticizer as the ability to absorb the polymer content. The rheological properties of the SCC were examined in various mixing time and temperature. After changing the temperature of the SCC to the ambient temperature, the rheology test was conducted using rheometer in 60 min. In this research, the dosage of rheological parameters and its growth rate with time have been compared in various temperatures. According to the obtained results, Naphthalene sulfonate cause to increase yield stress and to decrease plastic viscosity more than poly-carboxylate in SCC, in other words, poly-carboxylate cause better viscosity in concrete. Also, concrete containing naphthalene sulfonate has less yield stress growth rate and viscosity by increasing the time. On the other hand, slump loss of the SCC containing naphthalene sulfonate is less than the one containing poly-carboxylate. That is to say, naphthalene sulfonate protects the fluidity more than poly-carboxylate in SCC.}, keywords = {Self-consolidating concrete,Temperature,Rheology,polycarboxylate,naphthalene sulfonate}, title_fa = {بررسی اثر فوق روان کننده ها بر رئولوژی بتن خودتراکم برای زمان ها و دماهای مختلف}, abstract_fa = {در طرح مخلوط بتن خودتراکم، عملکرد فوق روان کننده ها به‌شدت تحت تأثیر دمای محیط قرار دارد؛ این موضوع به علت آن است که درجه حرارت وابسته به سرعت هیدراسیون، بر نرخ جذب فوق روان کننده به مخلوط بتن خودتراکم تأثیر می‌گذارد. در این تحقیق دمای مخلوط های بتن با توجه به شرایط محیطی فصل‌های مختلف انتخاب شده است. بنابراین پس رساندن دمای بتن به دمای محیط، خواص رئولوژی بتن تازه خودتراکم حاوی پلی کربوکسیلات و نفتالین سولفونات به‌عنوان یک تابع از زمان اختلاط، دما و مقدار مواد افزودنی با نسبت آب به سیمان 42/0، مورد بررسی قرار گرفته است. بر اساس نتایج به‌دست‌آمده از تنش جاری شدن و لزجت پلاستیک حاصل از دستگاه رئومتر در طول زمان 60 دقیقه، پلی‌کربوکسیلات نسبت به نفتالین سولفونات سبب بهبود رئولوژی یعنی تنش جاری کمتر و لزجت پلاستیک بیشتر می‌شود ولی با این وجود، ازآنجایی‌که نفتالین سولفونات سبب افت اسلامپ کمتر می‌شود بنابراین با استناد به این امر، نفتالین سولفونات سبب حفظ سیالیت بیشتری می‌شود. همچنین با استناد به نتایج تحقیق، باید برای بهبود رئولوژی از بالا رفتن دمای بتن و زمان بتن ریزی کاست، زیرا در غیر این صورت، باعث سخت شدگی بتن و درنتیجه کاهش رئولوژی می‌شود.}, keywords_fa = {بتن خودتراکم,دما,رئولوژی,پلی کربوکسیلات,نفتالین سولفونات}, url = {https://jcr.guilan.ac.ir/article_4052.html}, eprint = {https://jcr.guilan.ac.ir/article_4052_e947f96d99a5f0934b25e79072c33268.pdf} } @article { author = {Zareian, Mohammad Sajjad and Esfahani, Mohammad Reza and Hosseini, Abdollah}, title = {Experimental study of post-tensioned hybrid coupled wall system with friction devices at the beam-to-wall connection region}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {13-26}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.13756.1377}, abstract = {Post-tensioned coupled shear wall system is a new type of seismic lateral force resisting systems with self-centering capability. In this system, the coupling beam is not embedded into the walls, and coupling of concrete walls is achieved by posttensioning beam to the walls using unbonded post-tensioning (PT) strands. In this research, the cyclic behavior of post-tensioned steel coupling beam with friction devices at the beam-to-wall connection region is experimentally evaluated. Three 2/3-scale specimens were tested subjected to quasi‐static lateral loading. The specimens consisted of one control specimen without energy dissipation system and two specimens equipped with friction devices with different levels of damper normal force. Friction devices are used at the beam-to-wall connections to slip and dissipate the seismic input energy. The test results revealed that the specimens equipped with friction devices have excellent lateral stiffness, strength, and ductility, and have significant energy dissipation capacity and negligible residual displacements under reversed cyclic loading. In addition, the specimens is able to tolerate large nonlinear rotations without significant damage in the beam and the wall region. Adding friction devices increased the load-carrying capacity by 47% to 62% and significantly increased the energy dissipation capacity of the specimens. With a 30% increase in the damper normal force, the load capacity increased by about 10%, the average relative energy dissipation ratio by about 15% and the mean cumulative energy dissipation capacity by about 33%.}, keywords = {Hybrid coupled wall,Post tensioning,Residual displacement,Friction device,Cyclic Behavior}, title_fa = {بررسی آزمایشگاهی سیستم دیوار همبسته دوگانه پس‌کشیده مجهز به ادوات اصطکاکی در ناحیه اتصال تیر به دیوار}, abstract_fa = {سیستم دیوار بتنی همبسته دارای مقاومت، سختی و شکل‌پذیری مطلوبی می‌باشد و به عنوان یک سیستم سازه‌ای مناسب برای ساختمان‌ها مورد توجه است. با این حال این سیستم سازه‌ای همچون سایر سیستم‌های متعارف، بعد از زلزله‌های بزرگ متحمل تغییرشکل‌های ماندگار شده که منجر به عملیات تعمیر و بهسازی گسترده و هزینه‌بری می‌شود. سیستم دیوار همبسته دوگانه پس‌کشیده از جمله سیستم‌های لرزه‌ای جدیدی است که دارای قابلیت مرکزگرایی می‌باشد. در این سیستم، تیر همبند در دیوار فرو نمی‌رود و همبندی دیوارهای بتنی به وسیله‌ی پیش‌تنیده کردن تیر همبند با کابل‌های پرمقاومت انجام می‌شود. در این تحقیق به بررسی آزمایشگاهی رفتار تیر همبند فولادی پس‌کشیده مجهز به ادوات استهلاک انرژی اصطکاکی در ناحیه اتصال به دیوار بتنی پرداخته می‌شود. سه نمونه با مقیاس 2⁄3 تحت بار چرخه‌ای شبه‌استاتیکی مورد آزمایش قرار گرفت. نمونه‌ها شامل یک نمونه‌ کنترلی فاقد سیستم استهلاک انرژی و دو نمونه مجهز به ادوات اصطکاکی با سطوح مختلف پیش‌تنیدگی بود. ادوات اصطکاکی در ناحیه اتصال تیر به دیوار به منظور استهلاک انرژی مورد استفاده قرار گرفتند. نتایج نشان داد نمونه‌های مجهز به ادوات اصطکاکی توانایی تحمل تغییرشکل‌های غیرخطی بزرگ، بدون تغییرشکل ماندگار و بدون خسارت قابل ملاحظه در سیستم را دارند و رفتار لرزه‌ای پایداری تا دریفت 8% ارائه می‌دهند. افزودن ادوات اصطکاکی سبب افزایش 47% تا 62% ظرفیت باربری و افزایش قابل‌توجه ظرفیت استهلاک انرژی نمونه‌ها شده است. با افزایش 30% در نیروی پیش‌تنیدگی ادوات اصطکاکی، ظرفیت باربری حدود 10%، میانگین نسبت استهلاک انرژی نسبی حدود 15% و میانگین ظرفیت استهلاک انرژی تجمعی حدود 33% افزایش یافته است.}, keywords_fa = {دیوار همبسته دوگانه,پس‌کشیدگی,جابجایی ماندگار,وسایل اصطکاکی,رفتار چرخه‌ای}, url = {https://jcr.guilan.ac.ir/article_4053.html}, eprint = {https://jcr.guilan.ac.ir/article_4053_d17fa0283bae7a16344ea36cea2cdeba.pdf} } @article { author = {Ebadi Jamkhaneh, Mehdi and Ahmadi, Masoud and Kheyroddin, Ali}, title = {Investigation of Seismic Performance of Concrete Bridge Piers Retrofitted by Steel Jacketing}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {27-38}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2019.6231.1151}, abstract = {One of the most useful methods for improving the seismic performance of concrete columns with insufficient shear strength is the use of a steel plate around the concrete column which by decreasing the crack and direct effect on shear force tolerance lead to improve the seismic performance. In this paper, the seismic behavior of specimens under cyclic loads was investigated in terms of force-displacement behavior, energy absorption and ductility. In this regard, the finite element method was used in OpenSEES program. At first, an experimental specimen was used to validate the numerical model and then, numerical model of the finite element was developed after proper matching of the responses with the experimental model and assurance of the type of loading, displacement boundary conditions, and the type of applied elements. The main parameters in these studies were the thickness of the steel jacketing, the spacing between the stirrups and the compressive strength of the concrete. The results of numerical studies showed that in the case of use of low strength concrete and the minimum thickness of steel plate, energy absorption, ductility and maximum load-bearing capacity can be 4.40, 1.66 and 2.5 times higher than reference model.}, keywords = {Rehabilitation,Steel jacket,Ductility,Cyclic Loading}, title_fa = {بررسی عملکرد لرزه ای پایه های پل بتن آرمه تقویت شده با جدار فولادی}, abstract_fa = {در این مقاله، رفتار لرزه ای ستون های بتنی تحت بارهای چرخه ای در قالب رفتار نیرو-تغییرمکان، میزان جذب انرژی و شکل پذیری مورد بررسی قرار گرفت. در این راستا از روش المان محدود در برنامه ی اپنسیس استفاده شد. ابتدا از مدل آزمایشگاهی جهت اعتبارسنجی مدل عددی استفاده شد و پس از تطبیق مناسب پاسخ های مدل عددی با مدل آزمایشگاهی و اطمینان از اعمال نوع بارگذاری، شرایط مرزی نیرویی و تغییرمکانی و نوع المان های بکار گرفته شده، مدل عددی المان محدود بسط داده شد. متغیرهای اصلی در این مطالعات ضخامت روکش های فولادی، فاصله ی بین خاموت های عرضی و مقاومت فشاری بتن بودند. نتایج مطالعات عددی نشان داد که در صورت استفاده از بتن با مقاومت پایین و کمترین ضخامت جدار فولادی، جذب انرژی، شکل پذیری و حداکثر ظرفیت باربری را می توان 4.4 برابر، 1.66 برابر و 2.5 برابر نسبت به نمونه ی مرجع نمود.}, keywords_fa = {بهسازی,جدار فولادی,شکل پذیری,بارگذاری چرخه ای}, url = {https://jcr.guilan.ac.ir/article_3744.html}, eprint = {https://jcr.guilan.ac.ir/article_3744_2fa7fd3b7ebb750d3d3a44edec379748.pdf} } @article { author = {Ghasemzadeh Mosavi Nejad , Seyed Hosein and Ramezani Khajeh Ghiyasi, Mohamad}, title = {The influence of Crystalline Admixture on the Self healing Concrete}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {39-51}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.12357.1338}, abstract = {Cracking on the concrete surface reduces the durability of the materials. The penetration of water and harmful chemicals through these cracks into concrete will cause corrosion of rebar and demolition of concrete. If we can prevent the development of small cracks when it occurs, we have prevented the creation of larger cracks, because of stress concentration. A hopeful way, is to add the agents that can heal concrete when cracks are occurred, are so called Self-healing concrete. The aim of this study is to analyze the self-healing effect of a crystalline admixture (4% by the weight of cement) in three types of environmental exposure comparing with a reference concrete. Healing was studied by means of permeability tests on cracked specimens and physical closing of the crack was observed by optic microscope and quantified through crack geometrical parameters. The studied crack openings were under 400 µm and the time set for healing was 42 days. The results show a different healing behavior depending on the exposure and the presence of the crystalline admixture, demonstrating that the presence of water is necessary for the healing reactions. Moreover, the respective rate of self-healing for all specimens at three different environmental conditions were obtained approximately 0.85 for the sinking in water, 0.59 for alternate wetting and drying and -0.265 for drying conditions.}, keywords = {concrete,self healing,crystalline admixture,Durability,permeability}, title_fa = {تاثیر مواد افزودنی کریستال شونده بر خود ترمیمی بتن}, abstract_fa = {ترک خوردگی در سطح بتن موجب کاهش دوام مصالح می گردد. بنا براین، با جلوگیری از توسعه ترک‌های کوچک در هنگام وقوع آن از به وجود آمدن ترک‌های بزرگ تر پیشگیری می‌شود. یک روش افزودن موادی است که بتن بتواند در هنگام ایجاد ترک، خودش را ترمیم کند. هدف اصلی بررسی تاثیر مواد افزودنی کریستالی شونده (4% وزن سیمان)، بر خودترمیمی بتن در سه شرایط محیطی و مقایسه آن با بتن شاهد است. ترمیم به وسیله آزمایش نفوذپذیری بر روی نمونه‌های ترک خورده مختلف بررسی گردید و بسته‌شدگی فیزیکی ترک توسط میکروسکوپ نوری و با استفاده از پارامتر‌های هندسی ترک اندازه‌گیری شد. بازشدگی ترک‌های بررسی شده زیر 400 میکرومتر است و برای این ترک‌ها به مدت 42 روز فرصت ترمیم در نظر گرفته شد. نتایج نشان می‌دهد که ترتیب نرخ ترمیم برای همه نمونه‌ها در سه شرایط محیطی غوطه‌ور در آب(نزدیک 85/0)، تر و خشک شدن‌های متناوب(نزدیک 59/0)و خشک(نزدیک 265/0-) بدست آمد.}, keywords_fa = {: بتن,خودترمیم,مواد افزودنی کریستال شونده,دوام,نفوذپذیری}, url = {https://jcr.guilan.ac.ir/article_4054.html}, eprint = {https://jcr.guilan.ac.ir/article_4054_6e7157cd2e0431dcf7c8af3725a37118.pdf} } @article { author = {abdolrasool, alireza and Mousavi, S. Yasin}, title = {Effects of wollastonite powder on the fresh properties of self-compacted concrete}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {53-65}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.13137.1362}, abstract = {The use of mineral additions in self-compacting concrete (SCC) as a substitute for Portland cement can not only improve the engineering properties and durability of concrete, but also reduce the environmental impacts of cement production. Nonetheless, due to the high sensitivity of SCC to its constituent materials, an appropriate study on the performance of mineral additions in the production of SCC is absolutely essential. The purpose of this study was to evaluate the fresh properties of SCC containing wollastonite powder in comparison with silica fume and natural zeolite. In this respect, 18 SCC mixtures were designed in four groups with different water/binder ratio and additions contents. Immediately after mixing, the fresh properties of concrete mixtures were evaluated for slump flow, visual stability index, T50, V-funnel time, J-ring and the sieve stability index. The results revealed that although, regardless of the water/binder ratio, the incorporation of wollastonite decreases the slump flow diameter, it can reduce the demand for high-range water reducer admixture usage in comparison with natural zeolite and silica fume. Also, the increase in viscosity and passing ability improvement were observed when wollastonite is used in SCC. Sieve stability index indicated a good segregation resistance in the presence of wollastonite.}, keywords = {Self-compacted concrete,wollastonite,traditional additions,Workability}, title_fa = {تاثیر پودر ولاستونیت بر خواص بتن تازه خودتراکم}, abstract_fa = {استفاده از افزودنی های معدنی در بتن خودتراکم به عنوان جایگزین بخشی از سیمان نه تنها می تواند خواص مهندسی و دوام بتن را بهبود بخشد، بلکه در کاهش اثرات زیست محیطی ناشی از تولید سیمان موثر می باشد. با اینحال، با توجه به حساسیت بالای بتن خودتراکم نسبت به مواد تشکیل دهنده آن، مطالعه دقیق عملکرد افزودنی های معدنی در ساختار بتن خودتراکم امری کاملا ضروری است. هدف از انجام این مطالعه ارزیابی خواص بتن تازه خودتراکم حاوی پودر ولاستونیت در مقایسه با دوده سیلیس و زئولیت می باشد. لذا 18 اختلاط بتن خودتراکم در چهار گروه با نسبت های مختلف آب به چسباننده و میزان افزودنی طراحی و تولید شد. بلافاصله پس از ساخت مخلوط های بتن خودتراکم، خواص بتن تازه توسط جریان اسلامپ، شاخص پایداری چشمی، زمان رسیدن جریان اسلامپ به قطر 50 سانتیمتر (T50)، قیف V شکل، حلقه J و شاخص الک پایداری ارزیابی شد. نتایج بتن تازه خودتراکم نشان می دهد هرچند صرفنظر از میزان آب به چسباننده، استفاده از ولاستونیت سبب کاهش میزان جریان اسلامپ می گردد، ولاستونیت در مقایسه با زئولیت و دوده سیلیس تقاضا برای مصرف کاهنده شدید آب را کاهش داده است. همچنین افزایش لزجت و بهبود قابلیت عبورکنندگی در صورت استفاده از ولاستونیت در بتن خودتراکم مشاهده شد. نتایج شاخص الک پایداری نیز نشان از مقاومت مطلوب در برابر جداشدگی در صورت حضور ولاستونیت در بتن خودتراکم دارد.}, keywords_fa = {بتن تازه خودتراکم,ولاستونیت,افزودنی های متداول,کارایی}, url = {https://jcr.guilan.ac.ir/article_4050.html}, eprint = {https://jcr.guilan.ac.ir/article_4050_d60a71eff3bdc3eb73ce641bb4e8f455.pdf} } @article { author = {Darvishan, Ehsan}, title = {Prediction of the Lateral Confinement Coefficient of The concrete Columns Confined by FRP using the Artificial Neural Network}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {67-80}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.12174.1335}, abstract = {Confining columns is one of the most commonly used methods of retrofitting structures. The confinement of concrete columns by FRP sheets is considered as one of the modern methods of retrofitting structures due to their properties. Tests conducted on a rounded-corner column by applying axial compression indicate that its behavior improves as well as the cross-section of column approaches the circular section. However, the behavior of columns confined with FRP or having transverse reinforcement has been studied by many researchers, yet study on wrapping columns by FRP when the transverse reinforcement does not satisfy the required confinement for the column has not been investigated by researchers. In this study, different models of the lateral confinement coefficient are presented. Also, by considering valid test results and the influence of different parameters such as length and width of column section, thickness of FRP sheet, the compressive strength of concrete, elasticity modulus of FRP and, radius of rounded-corner concrete a new model is presented using the Neural network in which the lateral confinement coefficient of confined columns can be predicted with high accuracy. Finally, the sensitivity analysis is carried out to evaluate the effect of each input parameter on the output parameter, and the results are presented.}, keywords = {Retrofitting,Reinforced Concrete Column,FRP,Artificial neural network,Confinement}, title_fa = {پیش ‏بینی ضریب محصور‏شدگی جانبی ستون ‏های بتنی محصور شده با FRP به وسیله‏ شبکه عصبی مصنوعی}, abstract_fa = {محصور نمودن ستون یکی از پرکاربردترین روش‏های مقاوم‏سازی ساختمان محسوب می‏شود. محصور نمودن ستون‏های بتنی با ورقه‏های FRP به دلیل ویژگی‏هایی که دارد از جمله روش‏های نوین مقاوم‏سازی سازه‏ها محسوب می‏گردد. آزمایش‏هایی که با اعمال فشار محوری به ستون‏های دارای گردگوشگی انجام گرفته است، نشان می‏دهد که هرچه ستون به مقاطع دایره‏ای نزدیک‏تر شود، رفتار آن بهبود می‏یابد. اگر‏چه رفتار ستون‏‏های بتن‏آرمه محصور شده با FRP یا دارای آرماتور عرضی توسط پژوهشگران زیادی مورد مطالعه قرار گرفته است، اما تحقیق در مورد دورپیچ نمودن ستون با FRP زمانی که آرماتورهای عرضی پاسخگوی محصورشدگی مورد نیاز ستون نیستند، کمتر مورد توجه قرار گرفته است. در این مقاله مدل‏های مختلفی از ضریب محصورشدگی جانبی ارائه شده است همچنین با در نظر گرفتن نتایج 114 آزمایش معتبر و تاثیر پارامترهای مهمی از جمله طول و عرض مقطع ستون، ضخامت ورق FRP، مقاومت فشاری بتن، مدول الاستیسیته FRP و شعاع گردشدگی گوشه‏های بتن، مدل جدیدی با استفاده از شبکه عصبی ارائه شده است که با استفاده از آن می‏توان ضریب محصورشدگی جانبی ستون‏های محصور شده را با دقت بالایی پیش‏بینی کرد. در نهایت، آنالیز حساسیت به منظور بررسی میزان تاثیر هر پارامتر ورودی روی پارامتر خروجی نیز انجام گرفته و نتایج آن ارائه شد. با توجه به دقت بالای مدل پیشنهادی توسط شبکه عصبی بدین ترتیب برای محاسبه ضریب محصورشدگی جانبی ستونی که پارامترهای آن در بازه پارامترهای تعریف شده در این مطالعه باشد دیگر نیازی به صرف هزینه و زمان برای مطالعه آزمایشگاهی آن ستون نمی‏باشد.}, keywords_fa = {مقاوم سازی,ستون بتن آرمه,FRP,شبکه عصبی مصنوعی,محصورشدگی}, url = {https://jcr.guilan.ac.ir/article_4028.html}, eprint = {https://jcr.guilan.ac.ir/article_4028_bec9d35a7a6e7ba842f0105861381105.pdf} } @article { author = {pachideh, ghasem and gholhaki, majid and moshtagh, amin}, title = {Laboratory study of mechanical properties and microstructure of cement mortar containing Silicafume and Granulated Blast- Furnace Slag in post-high temperature conditions}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {81-97}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.12238.1334}, abstract = {Sandstone shrinks on heating, and therefore, it counteracts to some extent the expansion of the quartz grains. The loss in strength of sandstone mortars on exposure to fire is, however, often high, and therefore sandstone does not form a good fire-resistant aggregate. This paper deals with an experimental study on the post-heat performance of cement mortars containing silica fume and granulated blast-furnace slag (GBFS). In doing so, the mortar specimens were provided in standard formworks to perform compressive, tensile and flexural tests containing 7, 14 and 21% of pozzolanic materials as a replacement for cement. Moreover, for the sake of heating process, the specimens were placed in an electric furnace exposed to temperatures of 25, 100, 250, 500, 700 and 9000c with standard temperature increment and once the heating process ended and the specimens were cooled, the tests were carried out on them. Based on the results obtained, the maximum effect of utilizing granulated blast-furnace slag (GBFS) and silica fume respectively takes place in low (up to 2500c) and high (5000c and greater degrees) temperatures. Quantitatively, the compressive, tensile and flexural strengths were raised by 73 and 180%, 45 and 100%, 106 and 112%, respectively in low and high temperatures. In addition, as the temperature rises, the particles of specimens containing silica fume and granulated blast-furnace slag (GBFS) shrinks less in size compared to the reference specimen.}, keywords = {Cement Mortar,silica fume,granulated blast-furnace slag (GBFS),Heat,XRD Analysis}, title_fa = {مطالعه آزمایشگاهی خواص مکانیکی و ریزساختار ملات سیمانی حاوی پودر میکروسیلیس و سرباره کوره‌آهن‌گدازی در شرایط پس از دماهای بالا}, abstract_fa = {در این مقاله به مطالعه آزمایشگاهی عملکرد پس از حرارت ملات‌های سیمانی حاوی میکروسیلیس و سرباره کوره آهن‌گدازی پرداخته شد. بدین منظور نمونه‌های ملات در قالب‌های استاندارد جهت انجام تست مقاومت فشاری، کششی و خمشی حاوی 7، 14 و 21 درصد پوزولان بعنوان جایگزین سیمان مصرفی ساخته شد. همچنین بمنظور انجام عملیات حرارتی، نمونه‌ها در کوره الکتریکی در دماهای 100، 250، 500، 700 و 900 درجه سانتی‌گراد با نرخ افزایش دمای استاندارد قرار گرفته و پس از اتمام فرآیند حرارت‌دهی و سرد‌شدن نمونه‌ها، آزمایشات لازم بر روی هر یک انجام شد. نتایج نشان داد که بیشترین تأثیر استفاده از سرباره کوره آهن‌گدازی و میکروسیلیس به ترتیب در دماهای پایین (تا 250 درجه سانتی‌گراد) و دماهای بالا (500 درجه سانتی‌گراد و بالاتر) با رشد 73% و 180% مقاومت فشاری، 45% و 100% مقاومت کششی و 106% و 112% مقاومت خمشی قابل مشاهده است. همچنین با افزایش دما، اندازه دانه نمونه‌های حاوی میکروسیلیس و سرباره کوره آهن‌گدازی در آزمایش XRD، دچار افت کمتری تا حدود 6 درصد نسبت به نمونه شاهد شده است.}, keywords_fa = {ملات سیمانی,میکروسیلیس,سرباره کوره آهن‌گدازی,حرارت,آزمایش XRD}, url = {https://jcr.guilan.ac.ir/article_4049.html}, eprint = {https://jcr.guilan.ac.ir/article_4049_661a3b5f0d5b60af8e8f5cf3c752e514.pdf} } @article { author = {kiamarsi, arman and Jabbari, Mohammad Mahdi}, title = {The effect of using Polymeric Wastes UPVC on mechanical properties of concrete}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {99-112}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.12658.1345}, abstract = {The mass production and distribution of plastic materials in the 1950s was one of the major achievements of mankind, that currently the human needs it as an important industry for many reasons like variety, inexpensive and availability. The environmental damage caused by fossil contaminants, the consumption of some communities and the release of them and the lack of knowledge after the end of their initial consumption period is irrational and in the medium and long time, there will be imposed heavy costs. In this research, the effect of the mixing of polymeric waste (UPVC) are reviewed in the two forms of fibers and grains and in various volumetric percentages (0, 2.5, 5, 7.5 and 10% for fiber form) and (0, 5, 10 and 15% for the grain form) in order to replace the sand in the construction of concrete and the experiments carried out such as compressive strength, tensile strength, flexural strength, and fresh concrete tests, such as slump and concrete specific gravity. The ratio of water to cement was fixed (0.45) in all mixtures and the processing of 7 and 28-days of the samples was performed according to standard laboratory conditions. The results of this study indicate that the use of these wastes in concrete improves heat resistance and up to 5% for fiber form and up to 10% for grain form has a slight reduction in the mechanical properties and specific gravity of the concrete and it improves tensile and flexural strength.}, keywords = {UPVC waste,concrete,compressive strength,Tensile strength,Flexural strength}, title_fa = {تاثیر استفاده از ضایعات پلیمری UPVC بر خواص مکانیکی بتن}, abstract_fa = {تولید و عرضه گسترده مواد پلاستیکی در دهه 50 میلادی یکی از دستاوردهای مهم بشر بود که امروزه بدلیل گوناگونی و تنوع، ارزان و در دسترس بودن، به عنوان صنعتی مهم انسان را به خود وابسته کرده‌اند. آسیب‌های زیست‌محیطی ناشی از آلاینده‌های فسیلی، مصرف‌گرایی برخی جوامع و رها‌سازی و بی‌ارزش دانستن بعد از اتمام دوره مصرف اولیه آنها، روشی غیرمنطقی بوده و در افق میان مدت و بلند مدت، هزینه‌های تحمیلی سنگینی نیز به همراه خواهد داشت. در این پژوهش، اثر اختلاط ضایعات پلیمری یو‌پی‌وی‌سی در دو شکل الیاف و دانه‌ای و در درصدهای حجمی مختلف (0، 5/2 ، 5، 5/7 و 10 درصد برای شکل الیاف) و (0، 5، 10 و 15 درصد برای شکل دانه‌ای)، جایگزین ماسه در ساخت بتن و انجام آزمایش‌هایی چون مقاومت فشاری، مقاومت کششی، مقاومت خمشی و آزمایش‌های بتن تازه نظیر اسلامپ و وزن مخصوص بتن، در دستور کار قرار گرفت. نسبت آب به سیمان در تمامی اختلاط‌ها ثابت (45/0) و عمل‌آوری 7 و 28 روزه نمونه‌ها طبق شرایط استاندارد آزمایشگاهی انجام شد. نتایج حاصل از این پژوهش حاکی از آن است که استفاده از این ضایعات در بتن، تا 5 درصد برای شکل الیافی و تا 10 درصد برای شکل دانه‌ای، کاهش ناچیزی در خواص مکانیکی و وزن مخصوص بتن داشته و سبب بهبود مقاومت کششی و خمشی می‌شود.}, keywords_fa = {ضایعات یو‌پی‌وی‌سی,بتن,مقاومت فشاری,مقاومت کششی,مقاومت خمشی}, url = {https://jcr.guilan.ac.ir/article_4051.html}, eprint = {https://jcr.guilan.ac.ir/article_4051_14ba80ac5877630dc85c0346c91b6e0c.pdf} } @article { author = {salehizadeh, mohsen and Dizangian, Babak}, title = {Evaluation of strength of porous concrete made using scrap rubber}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {113-128}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.14440.1393}, abstract = {Porous concrete is one of the types of coatings used in rigid pavements. High porosity and good drainage efficiency have increased the use of this type of concrete in urban floods and runoff management. On the one hand, there is a large amount of corroded rubber produced annually in the world, which, due to the very slow rate of decomposition and contamination resulting from it, cannot be buried in the environment. The use of these worn-out tires in concrete is a good option to dispose of these wastes. In this study, experiments were conducted to investigate the effect of using scrap tires on the properties of porous concrete, and 5 modes of replacement of natural concrete aggregates with crumb rubber, including 5, 10, 15, 20 and 25 The percentage has been examined. The results show that replacement of crushed rubber and aggregates in porous concrete mixing design will reduce compressive and tensile strength. The effect of the presence of particulate rubber in the design of porous concrete mix on the reduction of tensile strength is more than its effect on the reduction of compressive strength. The results show that with increasing percentage of replacement of particulate rubber and aggregates in porous concrete, both porosity and permeability increase. Also, the compressive and tensile strength of specimens containing particulate rubber, after being placed in the sulfate medium, is lower than the compressive and tensile strength of the control sample}, keywords = {Porous concrete,compressive strength,Concrete Permeability,Concrete tensile strength,Crumb rubber}, title_fa = {ارزیابی مقاومت بتن متخلخل و ساخته شده با استفاده از خرده لاستیک ضایعات}, abstract_fa = {بتن متخلخل یکی از انواع پوشش‌های مورد استفاده در روسازی‌های صلب می‌باشد. تخلخل بالا و قابلیت زهکشی مناسب، کاربرد این نوع بتن را در مدیریت سیلاب‌ها و رواناب‌های مناطق شهری بطور موثری افزایش داده است. از سویی، سالانه در جهان مقدار زیادی لاستیک فرسوده تولید می‌شود، که به دلیل سرعت بسیار کم تجزیه و آلودگی‌های ناشی از آن، امکان دفن این لاستیک‌ها در محیط زیست وجود ندارد. استفاده از این لاستیک‌های فرسوده در بتن، به عنوان یک گزینه مناسب جهت دفع این ضایعات مطرح می‌باشد. با توجه به این موارد، در این تحقیق به منظور بررسی تأثیر استفاده از خرده لاستیک‌های ضایعاتی، بر خواص بتن متخلخل، آزمایشاتی انجام شده و 5 حالت جایگزینی سنگدانه‌های طبیعی بتن با خرده لاستیک، شامل 5، 10، 15، 20 و 25 درصد، مورد بررسی قرار گرفته است. بررسی نتایج نشان می‌دهد که جایگزینی خرده لاستیک و سنگدانه در طرح اختلاط بتن متخلخل، باعث کاهش مقاومت فشاری و کششی خواهد شد. بطوریکه اثر حضور خرده لاستیک در طرح اختلاط بتن متخلخل بر کاهش مقاومت کششی، بیشتر از اثر آن بر کاهش مقاومت فشاری می‌باشد . نتایج نشان می‌دهد که با افزایش درصد جایگزینی خرده لاستیک و سنگدانه در بتن متخلخل، درصد تخلخل و نفوذپذیری هر دو افزایش می‌یابند. همچنین مقاومت فشاری و کششی نمونه‌های حاوی خرده لاستیک، پس از قرارگیری در محیط سولفاتی، نسبت به مقاومت فشاری و کششی سولفاته نمونه شاهد، کمتر است.}, keywords_fa = {بتن متخلخل,مقاومت فشاری,نفوذپذیری بتن,مقاومت کششی بتن,خرده لاستیک}, url = {https://jcr.guilan.ac.ir/article_4055.html}, eprint = {https://jcr.guilan.ac.ir/article_4055_fd5e46dd4d789509af9e6364362f673c.pdf} } @article { author = {farokhzad, reza and jamali, mohammad}, title = {Effect of Xanthan gum Additive on Mechanical, durability properties of concrete}, journal = {Concrete Research}, volume = {13}, number = {1}, pages = {129-141}, year = {2020}, publisher = {University of Guilan}, issn = {2008-4242}, eissn = {}, doi = {10.22124/jcr.2020.13304.1367}, abstract = {Today, the use of powdered materials and chemical additives to improve the mechanical, durability, and rheological properties of a variety of concretes is rapidly expanding. The use of naphthalene, polycarboxylate and melamine-based lubricating and thickening agents is one of the effective strategies to control the instability of concrete. One of the foundations of the new lubricant is the xanthan gum biopolymer. The substance synthesized from the vegetable gum has a high viscosity that is widely used in various industries. After observing the lubricating type, high consistency, and appropriate price of this material, we decided to observe its effect on concrete. In this research, 16 mixing schemes containing Pozzolan Microsilica with 10 wt% cement and different grades were investigated. A 0.25 wt% lubricant and xanthan gum additive were added to the concrete cube samples. The results show that the xanthan gum additive reduces slump and separation and increases compressive strength, due to the increased viscosity. A bonding between concrete materials and decreased pores and porosity would reduce the capillary coefficient and increase electrical resistance of the concrete. Microstructural studies of concrete, including scanning electron microscopy (SEM) experiments, showed that the permeability is reduced and structural bonds of concrete adhesive are strengthened, due to the use of xanthan gum, and as a result, the samples containing xanthan gum have less porosity than samples lacking xanthan gum.}, keywords = {concrete,Xanthan gum,microstructural,Durability,Mechanical properties}, title_fa = {بررسی تاثیر ماده افزودنی زانتان گام بر خواص مکانیکی و دوام بتن}, abstract_fa = {امروزه استفاده از مواد پودری و افزودنی های شیمیایی، جهت ارتقاء خواص مکانیکی، دوامی و رئولوژیکی انواع بتن ها به شدت در حال گسترش است. استفاده از مواد روان‌ساز و قوام‌دهنده برپایه های مختلف( نفتالین، پلی‌کربوکسیلات و ملامین) یکی از راهکارهای موثر، جهت کنترل میزان ناپایداری بتن است. یکی از پایه های روان ساز و قوام بخش جدبد، بیوپلیمر زانتان گام می‌باشد. این ماده سنتز شده از صمغ گیاهی، دارای لزجت بالا بوده که در صنایع مختلف دارای کاربردهای فراوانی می باشد. پس از مشاهده نوع روانی، قوام بالا و قیمت مناسب این ماده برآن شدیم تاثیر آن را در بتن نیز مشاهده نماییم. در این تحقیق 16 طرح اختلاط حاوی پوزولان میکروسیلیس با 10 درصد وزنی سیمان و عیارهای مختلف سیمان مورد بررسی قرار گرفت. به نمونه های مکعبی بتنی، روان کننده به میزان 25/0 درصد وزنی و ماده افزودنی زانتان گام اضافه گردید. نتایج نشان می‌دهد که افزودنی زانتان گام به دلیل افزایش لزجت باعث افت اسلامپ، کاهش جداشدگی و افزایش مقاومت فشاری می گردد. ایجاد پیوستگی بین مصالح بتن و کاهش خلل و فرج و تخلخل، موجب کاهش ضریب موئینگی و افزایش مقاومت الکتریکی بتن می گردد. بررسی های ریزساختاری بتن، شامل آزمایش میکروسکوپ الکترونی روبشی(SEM) نشان داد، در اثر استفاده از زانتان گام، میزان نفوذپذیری کاهش و پیوندهای ساختاری چسب بتن تقویت گردیده و در نتیجه نمونه های حاوی زانتان گام، دارای تخلخل کمتری نسبت به نمونه‌های فاقد آن می‌باشد.}, keywords_fa = {بتن,زانتان گام,ریزساختار,دوام,خواص مکانیکی}, url = {https://jcr.guilan.ac.ir/article_4056.html}, eprint = {https://jcr.guilan.ac.ir/article_4056_0338d19bb00a8b25fec6ac6ad683cf54.pdf} }